Aggregation properties of amphiphilic poly(ethylene oxide)-poly(propylene oxide)-poly(ethylene oxide) block copolymer studied by cyclic voltammetry

โœ Scribed by Yuanhua Ding; Ying Wang; Rong Guo


Publisher
Springer-Verlag
Year
2004
Tongue
English
Weight
603 KB
Volume
7
Category
Article
ISSN
1097-3958

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Multi-Morphological Complex Aggregates F
โœ Yong Zhang; Zhijie Zhang; Qian Wang; Caihong Xu; Zemin Xie ๐Ÿ“‚ Article ๐Ÿ“… 2006 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 546 KB

## Abstract **Summary:** Amphiphilic triblock copolymers (PEO~__x__~โ€__b__โ€PDMS~__y__~โ€__b__โ€PEO~__x__~) with different block lengths were synthesized and multiโ€morphological complex crewโ€cut, starโ€like, and shortโ€chain aggregates were prepared by selfโ€assembly of the given copolymers. The morpholo

Preparation of gold nanosheets using pol
โœ Sang-Ho Cha; Jong-Uk Kim; Ki-Hyun Kim; Jong-Chan Lee ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 1009 KB

Gold nanosheets having single crystalline structure were successfully synthesized using the bulk phase mixture of HAuCl 4 and poly(ethylene oxide)-poly(propylene oxide)-poly(ethylene oxide) block copolymers through the irradiation of a glow lamp for 5 days. When the molar ratio of propylene oxide to

Solubilization of Gases by Poly(ethylene
โœ A.D. King Jr. ๐Ÿ“‚ Article ๐Ÿ“… 2001 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 66 KB

Measurements have been made to determine the solubilities of three hydrocarbon gases, methane, ethane, and propane, in aqueous solutions of four different water-soluble triblock copolymers of the Pluronic class: Pluronic P103, P104, P105, and F108. The solubilities of each gas, measured at 25 โ€ข C, f

Influence of poly(ethylene oxide)-poly(p
โœ Kerstin Drexler; Roland Meisel; Ingrid Grassert; Eckhard Paetzold; Hans Fuhrmann ๐Ÿ“‚ Article ๐Ÿ“… 2000 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 89 KB ๐Ÿ‘ 1 views

Suzuki reaction under phase transfer conditions: 15 mmol phenylboronic acid, 13 mmol p-iodoanisole, 0.01 mmol PdCl 2 [Ph 2 P(CH 2 ) 4 SO 3 K] 2 , 45 mmol Na 2 CO 3 in toluene/ethanol/water = 15 : 15 : 15 ml with 400 mg of different block copolymers; at 78 8C