Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle

✍ Scribed by Johannes Konnerth; Notburga Gierlinger; Jozef Keckes; Wolfgang Gindl


Publisher
Springer
Year
2009
Tongue
English
Weight
708 KB
Volume
44
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.

✦ Synopsis


Hardness and elastic modulus of spruce wood cell walls parallel to their axial direction were investigated by means of nanoindentation. In the secondary cell wall layer S2 of individual earlywood and compression wood tracheids, a systematic pattern variability was found. Several factors potentially affecting nanoindentation results were investigated, i.e. specimen orientation related to the indenter tip, cutting direction during specimen preparation, tip geometry, specimen and fibre inclination, respectively, and finally micro fibril orientation. Mechanical property measurements were correlated with structural features measured by confocal Raman spectroscopy. It was demonstrated that very high variability in the measurement of micromechanical cell wall properties can be caused by unintentional small fibre misalignment by few degrees with regard to the indentation direction caused by sub-optimal specimen preparation.