𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Active, passive and transpassive dissolution of a nickel base super alloy in concentrated acid mixture solution

✍ Scribed by Dr. V. B. Singh; U. Arvind


Publisher
John Wiley and Sons
Year
1995
Tongue
German
Weight
496 KB
Volume
46
Category
Article
ISSN
0947-5117

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

The electrochemical and corrosion behaviour of a nickel base super alloy (C‐263) has been investigated in the deaerated binary and ternary solution mixture of concentrated phosphoric acid, acetic acid, sulphuric acid, nitric acid or water using potentiostatic technique at 35°C. The possibilities of electropolishing of this alloy in these solution mixtures have been also explored. The alloy showed distinct active, passive and transpassive behaviour in the experimental solutions. The alloy remained active and turned passive in the negative potential region. Transpassive dissolution of the alloy is observed and electropolishing is achieved in this region. The best electropolishing is obtained in 50% H~3~PO~4~ + 40% CH~3~COOH + 10% H~2~SO~4~. Higher content of water in the electrolytic solution is not useful for electropolishing of the alloy The experimental results also suggest that a current plateau in the transpassive potential region is not a sufficient condition to achieve electropolishing.