The thermal degradation of cotton fibres treated with sodium hydroxide VC, max,
Acetylation of cotton treated with sodium hydroxide
✍ Scribed by S. H. Zeronian
- Publisher
- John Wiley and Sons
- Year
- 1970
- Tongue
- English
- Weight
- 448 KB
- Volume
- 14
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
The reactivity of mercerized, ethanol‐washed, never‐dried cotton, as indicated by acetylation, is higher than that of mercerized, water‐washed, never‐dried cotton. Hygroscopicity measurements indicate that the ethanol‐washed cotton is not fully amorphous. They also reveal that the accessibility of cotton treated with caustic soda solution of mercerizing strength will be higher than that of cotton treated with ethylamine regardless of whether water or a solvent of lower hydrogen‐bonding capacity is used to extract the swelling agent. Based on microscopic examination, acetylation of mercerized, ethanol‐washed fibers apparently takes place relatively uniformly. The breaking load of cotton fibers is similar to that of mercerized, ethanol‐washed cotton fibers of about 8% acetyl content. However, the crystallinity of these materials, as shown by hygroscopicity studies, is markedly different. This indicates that the fine structure of the cotton fiber can be modified considerably without causing a loss in strength. Yarn tensile tests indicate that mercerized, ethanol‐washed cotton yarn with acetyl content between 10% and 30% has a breaking load which is about 12% lower than that of cotton.
📜 SIMILAR VOLUMES
## Abstract The crystallite reorientation brought about by the swelling of cotton with sodium hydroxide solution (NaOH) has been investigated. The degree of reorientation as indicated by the decreased value of x‐ray angle may arise from deconvoluting and not necessarily from a change in orientation
Comparison was made for glyoxal-and glutaraldehyde-treated cotton fabrics. Crosslinking efficiency between cellulose and dialdehyde measured by wrinkle recovery angle was higher with glutaraldehyde than with glyoxal. This disparity was presumably due to different forms of two dialdehydes in aqueous