The authors have proved that ethylene-propylene rubber (EPR) is suitable for the solid electrical insulating material of superconducting and cryoresistive cables due to its excellent mechanical and good electrical properties. It is imperative to study the treeing resistivity of EPR in view of long-t
β¦ LIBER β¦
ac treeing of ethylene-propylene rubber in cryogenic temperature region
β Scribed by Atsushi Minoda; Yasuichi Mitsuyama; Yukio Mizuno; Masayuki Nagao; Masamitsu Kosaki
- Publisher
- John Wiley and Sons
- Year
- 1998
- Tongue
- English
- Weight
- 809 KB
- Volume
- 124
- Category
- Article
- ISSN
- 0424-7760
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
ac treeing of ethylene-propylene rubber
β
Atsushi Minoda; Yasuichi Mitsuyama; Yukio Mizuno; Masayuki Nagao; Masamitsu Kosa
π
Article
π
1998
π
John Wiley and Sons
π
English
β 189 KB
Tan Ξ΄ of ethylene-propylene rubber in cr
β
Yukio Mizuno; Yasuichi Mitsuyama; Atsushi Minoda; Masayuki Nagao; Masamitsu Kosa
π
Article
π
1996
π
John Wiley and Sons
π
English
β 804 KB
Cure characteristics of ethylene propyle
β
Abhik Sengupta; Bidyut Baran Konar
π
Article
π
1997
π
John Wiley and Sons
π
English
β 177 KB
π 2 views
Various blends of polypropylene and ethylene propylene diene terpolymer were prepared. In these blends, rubber phases were compounded with an optimum sulfur curing system. The equivalent cure time and state of cure of the mixes were studied in the temperature range from 120 to 190ΠC by a rheometer.