Modeling of the heat-transfer process in
โ
B. Sen
๐
Article
๐
1992
๐
American Institute of Chemical Engineers
๐
English
โ 546 KB
## Abstract The model developed predicts a priori potential errors associated with the energy trace recorded by an isoperibol differential power scanning calorimeter in the measurement of heat of adsorption of H~2~ on Pt and Pd catalysts. The uptake of H~2~ by the catalyst sample was approximated b