Improvement of pitting corrosion resista
β
T. Bellezze; G. Roventi; A. Quaranta; R. Fratesi
π
Article
π
2008
π
John Wiley and Sons
π
German
β 451 KB
π 1 views
## Abstract The pitting corrosion resistance of AISI 444, 304L and 316L stainless steels in two tap waters with different chloride concentrations at 80βΒ°C was studied. Cyclic potentiodynamic polarization (CPP) tests were carried out starting from __E__~corr~βββ30 mV until the current density reache