𝔖 Bobbio Scriptorium
✦   LIBER   ✦

A study of the pitting corrosion of cold-worked stainless steel

✍ Scribed by R. Štefec; F. Franz


Book ID
117087027
Publisher
Elsevier Science
Year
1978
Tongue
English
Weight
480 KB
Volume
18
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.