A small angle X-ray scattering study of carbons made from pyrolyzed sugar

✍ Scribed by A. Gibaud; J.S. Xue; J.R. Dahn


Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
481 KB
Volume
34
Category
Article
ISSN
0008-6223

No coin nor oath required. For personal study only.

✦ Synopsis


A small angle X-ray scattering study of carbons made from pyrolyzed sugar is presented. An analysis of the micropore size and surface area was performed as a function of the heat-treatment temperature between 600 and 2100Β°C. The observed X-ray data were analyzed using the model of Kalliat et al. [ 11, corrected for the experimental smearing function of the slits. The surface areas of the macro and micropores as well as the radius of gyration of the micropores were determined.


πŸ“œ SIMILAR VOLUMES


59. Small angle X-ray scattering from gl
✍ R.G Jenkins; P.L Walker Jr. πŸ“‚ Article πŸ“… 1973 πŸ› Elsevier Science 🌐 English βš– 128 KB

54. Optical reflectivity of a papbite single crystal\* E. S. Bomar and W. P. Eatherly (belay and Ceramics L&&ion, Oak Ridge ~at~~a~ ~~~at~, Oak Ridge, Ten~ssee). The reflectivity of a single crystal of Ticonderoga graphite was measured using a microscope photometer. The dependence of intensity on sa

Multiple X-ray small-angle scattering of
✍ R. Ferret; W. Ruland πŸ“‚ Article πŸ“… 1972 πŸ› Elsevier Science 🌐 English βš– 113 KB

Luzzati's method for the evaluation of multiple X-ray small angle scattering has been revised and completed. Under the usual experimental conditions multiple scattering occurs practically in all cases in which the produce of the average pore size (in A) and the volume fraction of pores is larger tha

Studies of fibrin film. II. Small-angle
✍ Fred J. Roska; John D. Ferry; J. S. Lin; John W. Anderegg πŸ“‚ Article πŸ“… 1982 πŸ› Wiley (John Wiley & Sons) 🌐 English βš– 759 KB

## Abstract Measurements of small‐angle x‐ray scattering have been made on bovine fibrin film, prepared by gentle compaction of coarse fibrin clots, containing 12–15% fibrin plasticized with either aqueous buffer or glycerol. Most of the experiments were made with water‐plasticized films because of