✦ LIBER ✦
A revised interpretation of ultra-fast stress corrosion cracking experiments by Serebrinsky and Galvele
✍ Scribed by Roger C Newman; Nicholas A. Senior
- Book ID
- 116385468
- Publisher
- Elsevier Science
- Year
- 2010
- Tongue
- English
- Weight
- 174 KB
- Volume
- 52
- Category
- Article
- ISSN
- 0010-938X
No coin nor oath required. For personal study only.