๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

A Phenomenological Model for Hydrogen Sulfide Stress Corrosion Cracking in Petroleum Tube Steels

โœ Scribed by V.D. Makarenko; V.A. Petrovskii; V.Yu. Chernov; I.O. Makarenko


Book ID
111575789
Publisher
Springer
Year
2004
Tongue
English
Weight
33 KB
Volume
40
Category
Article
ISSN
0009-2355

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES