𝔖 Bobbio Scriptorium
✦   LIBER   ✦

A novel method of electroless plating on AZ31 magnesium alloy sheet

✍ Scribed by Hui Zhao; Zhanghong Huang; Jianzhong Cui


Publisher
Elsevier Science
Year
2008
Tongue
English
Weight
775 KB
Volume
203
Category
Article
ISSN
0924-0136

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Effects of basal texture on mechanical b
✍ H. Wang; P.D. Wu; M.A. Gharghouri πŸ“‚ Article πŸ“… 2010 πŸ› Elsevier Science 🌐 English βš– 875 KB

The effect of the basal texture on the mechanical behaviour of AZ31B magnesium alloy sheet is studied numerically using a recently developed Elastic Visco-Plastic Self-consistent (EVPSC) model, in which both slip and twinning contribute to plastic deformation. We simulate uniaxial tension within the

Effects of strain rate, temperature and
✍ Tetsuo Naka; Takeshi Uemori; Ryutaro Hino; Masahide Kohzu; Kenji Higashi; Fusahi πŸ“‚ Article πŸ“… 2008 πŸ› Elsevier Science 🌐 English βš– 731 KB

Magnesium alloys usually exhibit low ductility at the room temperature due to its hexagonal close-packed structure, but it will be improved at elevated temperature. Therefore, warm press-forming of magnesium alloy sheets is quite attractive. In order to determine the optimum condition of press-formi

Preparation and characterization of inor
✍ S. Y. Zhang; Q. Li; X. K. Yang; H. X. Zhang; S. Y. Wang; F. Liu πŸ“‚ Article πŸ“… 2011 πŸ› John Wiley and Sons 🌐 German βš– 637 KB

## Abstract In this paper, a protective coating scheme was applied for the corrosion protection of AZ91D magnesium alloy. Electroless Ni coating (EN coating) as bottom layer, electrodeposited Ni coating (ENN coating), and silane‐based coating (ENS coating) as top layer, respectively, were successfu

Solidification of AZ31 magnesium alloy p
✍ Bong Sun You; Chang Dong Yim; Su Hyeon Kim πŸ“‚ Article πŸ“… 2005 πŸ› Elsevier Science 🌐 English βš– 948 KB

Magnesium plate of 120 mm width and 30 mm thickness was produced by horizontal continuous casting, and its microstructures were analyzed on the surface and in the plate interior. The defect formation on the surface and subsurface, such as side cracks, buckling, pores and segregation, was very sensit