✦ LIBER ✦
A non-isothermal differential scanning calorimetry method for the determination of specific surface energies in polymer crystals
✍ Scribed by A. Dobreva; M. Alonso; M. Gonzalez; A. Gonzalez; J.A. de Saja
- Publisher
- Elsevier Science
- Year
- 1995
- Tongue
- English
- Weight
- 366 KB
- Volume
- 258
- Category
- Article
- ISSN
- 0040-6031
No coin nor oath required. For personal study only.