𝔖 Bobbio Scriptorium
✦   LIBER   ✦

A nanoindentation technique for functional evaluation of cartilage repair tissue

✍ Scribed by Ebenstein, Donna M.; Kuo, Alfred; Rodrigo, Juan J.; Reddi, A. Hari; Ries, Michael; Pruitt, Lisa


Book ID
118060631
Publisher
Cambridge University Press
Year
2004
Tongue
English
Weight
856 KB
Volume
19
Category
Article
ISSN
0884-2914

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Nanoindentation differentiates tissue-sc
✍ Cheng Li; Lisa A. Pruitt; Karen B. King πŸ“‚ Article πŸ“… 2006 πŸ› John Wiley and Sons 🌐 English βš– 616 KB

## Abstract Cartilage mechanical properties are typically tested at the macroscale. To demonstrate the ability of nanoindentation to characterize __in situ__ articular cartilage properties at the tissue scale, we investigated the local structure–property relationships of intact articular cartilage