## Abstract An oroantral communication (OAC) is an open connection between the oral cavity and maxillary sinus. Closure of OACs is commonly performed with a surgical procedure using a mucoperiosteal flap. An alternative technique using synthetic biodegradable polyurethane (PU) foam for closure of O
A long-term in vitro biocompatibility study of a biodegradable polyurethane and its degradation products
✍ Scribed by B. van Minnen; B. Stegenga; M. B. M. van Leeuwen; T. G. van Kooten; R. R. M. Bos
- Publisher
- John Wiley and Sons
- Year
- 2005
- Tongue
- English
- Weight
- 274 KB
- Volume
- 76A
- Category
- Article
- ISSN
- 1549-3296
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
The biological safety of degradation products from degradable biomaterials is very important. In this study a new method is proposed to test the cytotoxicity of these degradation products with the aim to save time, laboratory animals, and research funds. A biodegradable polyurethane (PU) foam was subjected to this test method. The PU had soft segments of DL‐lactide/ϵ‐caprolactone and hard segments synthesized from butanediol and 1,4‐butanediiosocyanate. Copolymer foams without urethane segments, consisting of DL‐lactide/ϵ‐caprolactone, were tested as well. Accumulated degradation products were collected by degrading the foams in distilled water at 60°C up to 52 weeks. Cell‐culture medium was prepared from powder medium with this water. In different tests the cytotoxicity of this medium was established. The first signs of cytotoxicity were observed after 3–5 weeks of degradation. This accounts for both materials and reestablishes the good short‐term biocompatibility of these materials. The PU showed more toxicity toward the end stages of degradation in comparison with the copolymer. This is probably related to the accumulation of degradation products of the urethane segments. In the in vivo situation the degradation of the PU and the metabolism and excretion of degradation products may differ. Therefore, long‐term in vivo studies will have to establish whether these in vitro results are representative for the in vivo behavior of the degrading PU. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res, 2006
📜 SIMILAR VOLUMES
## Abstract Segmented poly(urethane urea)s (PUUs) with hard segments derived only from methyl 2,6‐diisocyantohexanoate (LDI) without the use of a chain extender have previously been described. These materials, which contain hard segments with multiple urea linkages, show exceptionally high strain c
## Abstract Biodegradable polyesterurethanes (PUs) may be used as scaffold materials for tissue regeneration applications, because of their excellent mechanical properties. In this study, the degradation of highly porous PU foams was evaluated __in vitro__. The PU had amorphous soft segments of DL‐
The present study investigated the in vitro mechanism and degradation rate of polyhydroxyoctanoate (PHO). Solution-cast PHO films were incubated in either water or isoosmotic phosphate-buffered saline (PBS) for periods ranging from 1 to 24 months. Physical characterization included weight loss, wate
## Abstract The use of ceramic‐on‐ceramic (alumina‐ and zirconia‐based) couplings in hip joint prostheses has been reported to produce lower wear rates than other combinations (i.e., metal‐on‐polyethylene and ceramic‐on‐polyethylene). The addition of zirconia into an alumina matrix (zirconia‐toughe
## Abstract We have developed a new 3D porous and biostable collagen scaffold for implantable glucose sensors. The scaffolds were fabricated around the sensors and crosslinked using nordihydroguaiaretic acid (NDGA) or glutaraldehyde (GA) to enhance physical and biological stability. The effect of t