๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

A Galvanic Corrosion Approach to Investigating Chromate Effects on Aluminum Alloy 2024-T3

โœ Scribed by Clark, William J.; Ramsey, Jeremy D.; McCreery, Richard L.; Frankel, Gerald S.


Book ID
118045617
Publisher
The Electrochemical Society
Year
2002
Tongue
English
Weight
241 KB
Volume
149
Category
Article
ISSN
0013-4651

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Effect of aging time and temperature on
โœ F. M. Khoshnaw; R. H. Gardi ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 141 KB ๐Ÿ‘ 1 views

## Abstract Two types of aluminum alloys, 2024โ€T3 and 7075โ€T6, have been selected in this study to investigate the effect of metallurgical aspects on exfoliation corrosion. To determine and evaluate the metallurgical effects of heat treatments on corrosion behaviour of these alloys, G34 ASTM test w