A fractographic study of stress corrosion cracking of Zircaloy-4 in a methanol/HCl solution
โ Scribed by Hong Moon-Hee; Pyun Su-Il; Chung Sung-Uk; Kim Jong-Sang
- Publisher
- Elsevier Science
- Year
- 1990
- Tongue
- English
- Weight
- 956 KB
- Volume
- 173
- Category
- Article
- ISSN
- 0022-3115
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
## Abstract Effect of specimen orientation, heat treatment and applied potential on the stress corrosion susceptibility of magnesium AZ61 (Mgโ6.3% Alโ0.5% Znโ0.20% Mn) alloy in an aqueous 3.5% NaCl + 2% K~2~CrO~4~ solution at room temperature was investigated. Stress corrosion times to failure were
## Abstract Localized corrosion morphologies of 2195 AlโLi alloy with various heat treatment in 4.0% NaCl solution (pH 6.5) were investigated, and its corrosion mechanism was studied using a threeโelectrode coupling system of ฮฑ (Al) substituting for the precipitateโfree zone (PFZ), simulated bulk ฮธ