A differential scanning calorimetry study of the thermal behavior of water-dipalmitoylphosphatidylcholine mixtures at subzero temperatures: Effects of water content, surface charge, and cholesterol
✍ Scribed by Jaap C. A. Offringa; Ron Plekkenpol; Daan J. A. Crommelin