Phase-field simulations of α →&#xa0
✍ H.M. Singer; I. Singer; A. Jacot 📂 Article 📅 2009 🏛 Elsevier Science 🌐 English ⚖ 664 KB

A phase-field model for the solid-solid a ? c transition of Ti-Al binary alloys is presented based on analytical Gibbs free energies and couplings to the thermodynamical database ThermoCalc. The equilibrium values recover the a + c phase boundaries. Morphological transitions from diffusive to massiv