𝔖 Bobbio Scriptorium
✦   LIBER   ✦

A differential scanning calorimeter for educational purposes

✍ Scribed by G. Van Der Plaats; L. Lutt; J. Van Der Plas; P. Theunissen; J. Zillekens


Publisher
Elsevier Science
Year
1989
Tongue
English
Weight
265 KB
Volume
151
Category
Article
ISSN
0040-6031

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Modeling of the heat-transfer process in
✍ B. Sen πŸ“‚ Article πŸ“… 1992 πŸ› American Institute of Chemical Engineers 🌐 English βš– 546 KB

## Abstract The model developed predicts a priori potential errors associated with the energy trace recorded by an isoperibol differential power scanning calorimeter in the measurement of heat of adsorption of H~2~ on Pt and Pd catalysts. The uptake of H~2~ by the catalyst sample was approximated b