๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

A computational model of the subcritical growth of stress-corrosion cracks in metallic plates

โœ Scribed by A. O. Sakara; Yu. V. Banakhevych


Book ID
106455466
Publisher
Springer
Year
2010
Tongue
English
Weight
765 KB
Volume
46
Category
Article
ISSN
1573-885X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


The significance of stress corrosion cra
โœ D. Rhodes; J.K. Musuva; J.C. Radon ๐Ÿ“‚ Article ๐Ÿ“… 1981 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 1005 KB

Abslraet-A model is proposed to account for interactions between fatigue and stress corrosion crack propagation mechanisms in appropriate corrosion fatigue conditions. Tests on an alloy steel, and both wrought and cast aluminium alloys, are reported. Despite the use of very simple coefficients in th