✦ LIBER ✦
A Comparison of the Growth Kinetics and Scale Morphology for Three Superalloys at 930°C in Air and Low PO2 Environments
✍ Scribed by F. Rabbani; L. P. Ward; K. N. Strafford
- Book ID
- 111535786
- Publisher
- Springer-Verlag
- Year
- 2000
- Tongue
- English
- Weight
- 179 KB
- Volume
- 54
- Category
- Article
- ISSN
- 0030-770X