A comparative pitting corrosion study of mild steel in different alkaline solutions containing salts with sulphur-containing anions

✍ Scribed by D.V. Vasquez Moll; R.C. Salvarezza; H.A. Videla; A.J. Arvia


Book ID
115846421
Publisher
Elsevier Science
Year
1984
Tongue
English
Weight
1009 KB
Volume
24
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Effect of amino acids containing sulfur
✍ Mohamed Samir S Morad; Abo El-Hagag A Hermas; Mohamed S Abdel Aal πŸ“‚ Article πŸ“… 2002 πŸ› Wiley (John Wiley & Sons) 🌐 English βš– 167 KB πŸ‘ 2 views

## Abstract Research on non‐toxic inhibitors is of considerable interest in investigations into the replacement of hazardous classical molecules. This paper reports the action of four amino acids containing sulfur on the corrosion of mild steel in phosphoric acid solution with and without Cl^βˆ’^, F^