𝔖 Bobbio Scriptorium
✦   LIBER   ✦

98/01925 Characterization of oils by differential scanning calorimetry : Aboul-Gheit, A. K. et al. Thermochim. Acta, 1997, 306, (1–2), 127–130


Publisher
Elsevier Science
Year
1998
Weight
212 KB
Volume
39
Category
Article
ISSN
0140-6701

No coin nor oath required. For personal study only.

✦ Synopsis


pressure of a hydrocarbon-alcohol blend can be lowered by adding a cosolvent for the hydrocarbon and the alcohol to the blend. The method is disclosed.

96AIl925 Characterization of oils by differential scanning calorimetry

Aboul-Gheit, A. K. er al. Thermochim. Acta, 1997, 306, (l-2), 127-130. Characterization of both lubricating and fuel oils is possible for lowtemperature specifications with better repeatability and reproducibility than the standard pour point and cloud point methods. These lowtemperature tests are non-destructive and can be followed by using the same sample for measuring the high-temperature thermal stability of the oil DSC (destructive test).